ABSTRACTThe Si3N4 ceramics(91wt%Si3N4+5wt%Y2O3+4wt%Al2O3) of room temperature strength 620--760 MPa and fracture toughness 7 MPa-m½ were prepared by microwave sintering and their microstructure and mechanical properties were studied.The experiment results show that the higher N2 pressure (>4atm) is very necessary for microwave sintering of Si3N4 ceramics; microwave sintering can greatly decrease the sintering temperature to 1500* C, and increase the transformation rate of α to β-Si3N4,and reduce the total sintering time to about 1 hour. The mechanical properties of the Si3N4 ceramics sintered by microwave are better than that by conventional pressureless sintering.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.