Abstract

The purpose of this study is to investigate the effect of the stearic acid as binder in sintering pure iron using a microwave furnace. The study was focused in mechanical properties such as porosity, density and micro-hardness of sintered product. The experiment was done by varying weight percentages of stearic acid and controlling the sintering parameters such as sintering temperature and sintering time. Increasing the percentage of stearic acid resulted in higher porosity and lower bulk density. Hardness has increased by increasing sintering temperature and sintering time. The optimum material properties were found at 1300 °C sintering temperature with addition 2 % stearic acid within 30 minutes sintering time.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.