Microwave processing of xPb(Mg1/3Nb2/3)O3–yPb(Zn1/3Nb2/3)O3–zPbTiO3 relaxor ferroelectric ceramics was investigated in a 2.45 GHz microwave radiation. The green compacts can be sintered to a density of higher than 98% theoretical with short soak time of 10–15 min at 960°C whereas 4 h of soak time was needed by conventional sintering to a comparable density. Smaller grain sizes and more uniform microstructure were developed due to volumetric heating and rapid sintering in microwave processing. Dielectric measurement showed microwave sintered samples could obtain comparable dielectric properties to the conventional sintered ones.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.