Abstract(NaY)1/2MoO4 was fabricated via the solid‐state reaction method of Na2CO3, Y2O3, and MoO3. Scanning electron microscopy results demonstrated that all the (NaY)1/2MoO4 ceramics could be densified well in the sintering temperature range of 900–960°C. Results of X‐ray diffraction analysis demonstrated that the (NaY)1/2MoO4 ceramics crystallized into tetragonal scheelite structure. Sintering (NaY)1/2MoO4 at 940°C for 2 h optimized the microwave dielectric properties of the ceramics. The microwave permittivity, Q × f, and TCF of the (NaY)1/2MoO4 were 10.9, 29 000 GHz and −40.7 ppm/°C, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.