Abstract
In this paper the powders of Zn1-xCoxO (x=0, 0.01, 0.02, 0.025, 0.05, 0.1) were fabricated by the conventional solid state reaction. The crystal structure was characterized by x-ray diffraction (XRD). The electromagnetic parameters were measured using vector network analyzer (VNA), the infrared emissivity in the wavelength range of 3-5μm and 8-14μm was measured by Dual-band infrared emissivity measuring instrument. The absorption bandwidth of the double-layer microwave absorber is obviously more than that of the single-layer absorber. The bandwidth of the double-layer microwave absorber for reflection loss R<-8dB is 2.64GHz over the range of 8.2-18GHz. The thickness of the absorbers is only 4 mm. The infrared emissivity is only 0.39 in the range of 3-5μm and 0.81 in the range of 8-14μm.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.