Abstract

Objectives: The aim of this study was to compare the microtensile bond strengths (µ TBS) of three core materials with one lithium disilicate reinforced ceramic using two resin cements.Methods: Three core materials (Nulite F® (Biodental Technologies), Filtek Z250® (3M-ESPE), Prettau-Anterior® (Zirkonzhan, Germany)) were prepared as blocks (10×10×4 mm3) according to the manufacturer’s instructions. Lithium disilicate ceramic blocks were also constructed and bonded to core specimens with two dual curing luting resin cements (Duo-Link® (Schaumburg, IL), Bifix QM® (VOCO, Cuxhaven, Germany)). Micro-bar specimens were prepared and loaded in tension to determine the µ TBS Failure modes were classified by scanning electron microscope (SEM). Data were analysed using two-way ANOVA and Tukey HSD test.Results: The µ TBS varied significantly depending on the core materials and resin cements used (P 0.05). The highest bond strength was obtained between zirconia core and Bifix QM (45.3 ± 6.7 MPa).Conclusion: In vitro µ TBS of glass ceramic blocks bonded to zirconia core material showed higher bond strength values than resin-based core material, regardless of the resin cement type used.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.