Abstract

Laser-surface alloying of titanium alloy Ti–6Al–4V with C and Si mixed powders has been carried out. The composite coatings, thickness of about 0.7 mm, mainly consisting of titanium carbides and silicides, have a hardness of about 1500 HV 0.1, and the wear resistance is 4 times more than that of the as-received.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.