Abstract

This work deals with the consolidation of a TiAl alloy powder by spark plasma sintering (SPS). Pre-alloyed powder with a composition of Ti–48Al–2Cr–2Nb (at.%) was consolidated in a SPS furnace at temperatures between 1200[Formula: see text]C and 1325[Formula: see text]C and with a pressure of 50 MPa. The microstructures obtained after SPS depend on the sintering temperature. Tensile tests at room temperature were performed. The alloy SPSed at temperatures not less than 1250[Formula: see text]C exhibits good properties at room temperature.