CaCu3Ti4O12 (CCTO) powder was synthesized by the combustion method. The effect of sintering temperature was studied on dielectric properties of the prepared ceramic samples. They have the dielectric constant of ~31 000 and 80 000 for the grain size of 0.3 and 30–100 μm. It is unusual for CCTO with a grain size of 0.3 μm to have a dielectric constant of ~31 000. Their giant dielectric constant could be explained by a two-step internal-barrier-layer-capacitor model, associated with grain boundaries and domain boundaries. The existence of domain boundaries helped to explain the contradiction of the dielectric mechanisms between polycrystalline and single-crystal CCTO.