Abstract

We have prepared thin La 1− x MnO 3 films by metal organic chemical vapour deposition. The films were grown at deposition temperature T D=700°C on various types of substrates; polycrystalline Al 2O 3, polycrystalline SrTiO 3 having various grain size, and single-crystalline SrTiO 3 slices. The films exhibited transition to metallic state at temperatures from 200 to 260 K, depending on the substrate. Resistivity at the transition ranged from the value of 10 Ω cm for the small grain size polycrystalline films to 100 and 300 mΩ cm for the large grain size polycrystalline and epitaxial film on the SrTiO 3 single-crystalline substrate, respectively. We discuss magnetoresistance in the La 1− x MnO 3 films in correlation with their microstructure, studied by transmission electron microscopy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.