Abstract

This study systematically investigated the low cycle fatigue deformation of a high Nb-containing TiAl alloy with a nominal chemical composition of Ti-45Al-8.5Nb-0.2W-0.2B-0.02Y at 850 °C by using transmission electron microscopy (TEM), scanning electron microscopy (SEM), and synchrotron-based high-energy X-ray diffraction (HE-XRD) techniques. Cyclic stress-strain (CSS) behavior, lattice strain, and peak broadening of {100}α2, {201}γ, and {202}ωo planes, phase transformations, and crack propagation behavior were obtained for samples with three total strain amplitudes: Δεt/2 = ±0.25%, Δεt/2 = ±0.28%, and Δεt/2 = ±0.30%. At early deformation stages, α2lamellae transformed into ωo phase with a distinct orientation relationship, and a certain orientation relationship (OR) between them was observed after the following cyclic deformation. Furthermore, γ particles precipitated within the single ωo area. In addition, according to the peak intensity and peak broadening results, the ωo → B2 phase transformation occurred, leading to the appearance of single B2-phase areas. The lattice strains in the ωo phase were always in tension during the cyclic deformation and large differences of the lattice strains were found in the γ phase and α2 phase, not only the values but also the directions, which resulted in crack nucleated at and propagated along the α2/γ lamellar interface. This study provides a better understanding of the low cycle fatigue deformation of TiAl alloys.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call