Abstract
ABSTRACTSlots with uneven width were cut by femtosecond laser in small plates of IN738LC superalloy to imitate service cracks. The ‘cracks’ were repaired by diffusion brazing using BNi-1a or a mixed filler alloy at 1100°C. The joint region was composed of isothermal solidification zone (ISZ), diffusion affected zone (DAZ) and precipitate zone (PZ). The compositions were different between the upper and lower ISZ due to the variation of gap width. The sample, repaired with two kinds of filler metals, had similar DAZ microstructure. PZ of mixed filler alloy bonded sample had a similar microstructure with that of BNi-1a, but less borides. The maximum gap sizes of complete isothermal solidification were almost the same for different filler alloys, followed a square root relationship with time. However, PZ of BNi-1a bonded was larger, resulting from a more base metal dissolution. The relationship between the PZ, ISZ and crack width is discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.