Abstract

The formation behavior of the fine-grain region alloyed with Zn due to diffusion induced recrystallization (DIR) in the Cu(Zn) system was experimentally examined for the surfaces polished in different manners using a Cu bicrystal containing a [1 1 0] twist boundary with a misorientation angle of θ = 46° zincified at 673 K for 2.88 × 104 s with Cu-15 wt% Zn and Cu-30 wt% Zn alloys by a capsule zincification technique. The extent and morphology of the fine-grain DIR region vary depending on the surface conditions and the composition of the Zn-source Cu-Zn alloy. For the specimen with the surface electrolytically polished in an etchant consisting of 20 vol% of nitric acid and 80 vol% of methanol, no DIR region was formed on the whole surface when the Cu-15 wt% Zn alloy was used as a Zn source.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.