Abstract
Herein, fiber laser welding experiments are performed to evaluate the microstructure, mechanical properties, and corrosion behavior of dissimilar/similar joints between DP980 and QP980 steel. Results show that the fusion zone (FZ) of all joints consists of lath martensite with high microhardness (≈480 HV); the retained austenite content in the subcritical heat‐affected zone (HAZ) in the QP980 side of the dissimilar weld joint (WJ) is less than base metals (BMs). Lower hardness in the subcritical HAZ is found compared with BMs in all joints. The microstructure of softening zones is tempered martensite, and the reduction in hardness is about 8.5−10.8% of BMs, which has a great influence on the tensile fracture position of WJs. All joints fracture at softening zones with a typical feature of ductile fracture, and the joint efficiencies are above 96%. The electrochemical corrosion test reveals that the welded samples exhibit a higher corrosion rate compared with the BMs due to the increase in martensite content and area fraction of grain boundary.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.