Abstract

AlSi7Mg0.6 alloys are directionally solidified with forced melt flow induced by a rotating magnet ring. By increasing the rotational frequency of the permanent magnet the columnar dendritic microstructure in the centre part of the samples changes completely towards a structure of small equiaxed grains with different crystallographic orientations, accompanied by an increased amount of eutectic and Mg2Si phases.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.