In the current investigation, the M2 high speed steel (HSS) sample was produced by laser direct metal deposition (DMD) with a rapid manufacturing (AM) process. The overall microstructure analysed by light optical microscopy (LOM) was a gradual transition from bottom zone to top zone due to the continuous decrease of the cooling rate. The observed microstructure from SEM and XRD was consisted of a cellular or dendritic structure of ferrite, martensite, retained austenite and fine carbides. Annealing at 860 oC led to spheroidization of carbides. The carbides were examined by XRD to be M6C and MC. With prolonging the annealing holding time, the more homogenous microstructure could be acquired. These studies demonstrated that annealing can improve microstructures of M2 HSS produced by DMD.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.