The microstructure evolution of Fe–30% Cu fine-grain composites during sintering of fine particle blends and during heat treatment of the high-density specimens up to 1130°C was investigated. The metal powder blends with particle sizes less than 0.1 μm were prepared by mechanical alloying technique. The quantitative analysis of microstructure was carried out. The microstructure of solid-state sintered composites was practically identical for all specimen treatment conditions and featured a high degree of dispersity and uniformity. Very fast coarsening of the microstructure took place at the temperature 1130°C during sintering powder blends and during heating of the high-density specimens. The mechanism of microstructure transformation is discussed. The solid-state treating Fe–30% Cu materials have high hardness and good conductivity after hardening. These characteristics impair immediately when the copper liquid-phase appears.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.