AbstractA new energy‐based quasicontinuum formulation is presented which is based on sampling the crystal energy at carefully‐chosen lattice sites and which allows for efficiently bridging from the atomistic to the continuum length scale. The presented technique is applied to experiments of nanoindentation whose microstructure‐induced size effects can now be studied with full atomistic detail at the micrometer scale without the necessity of phenomenological material models. (© 2013 Wiley‐VCH Verlag GmbH & Co. KGaA, Weinheim)
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.