Abstract

In as-cast Mg–2.1Gd–1.1Y–0.82Zn–0.11Zr (mole fraction, %) alloy, lamellar microstructures that extend from grain boundaries to the interior of α-Mg grains are identified as clusters of γ′ using a scanning transmission electron microscope equipped with a high-angle annular dark-field detector. Under a total strain-controlled low-cyclic loading at 573 K, the mechanical response and failure mechanism of Mg–2.1Gd–1.1Y–0.82Zn–0.11Zr alloy (T6 peak-aging heat treatment) were investigated. Results show that the alloy exhibits cyclic softening response at diverse total strain amplitudes and 573 K. The experimental observations using scanning electron microscopy show that the micro-cracks initiate preferentially at the interface between long-period stacking order structures and α-Mg matrix and extend along the basal plane of α-Mg. The massive long-period stacking order structures distributed at grain boundaries impede the transgranular propagation of cracks.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.