Abstract

Thermal deformation behavior of Cu-Cr-Sn alloy ingots under deformation temperatures ranging from 600 °C to 950 °C and strain rates from 0.01 s-1 to 10 s-1 was investigated in detail. The thermal deformation constitutive equation and thermal processing map of the alloy were established, respectively. The activation energy Q was determined as 430.61 KJ/mol. The optimal deformation system corresponding to the hot working diagram was a deformation temperature of 900 °C and strain rate of 0.1 s-1. Under these deformation conditions, twin dynamic recrystallization (TDRX), continuous dynamic recrystallization (CDRX), and discontinuous dynamic recrystallization (DDRX) occurred simultaneously, with the twinning process causing the stress-strain curve to exhibit a wavy change. The thermal deformation microstructure of the alloy is co-regulated by different recrystallization mechanisms, with DDRX occurring mainly at low deformation temperatures, and both CDRX and DDRX occurring at high deformation temperatures.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.