Abstract

Rheo-die casting (RDC) based on LSPSF (low superheat pouring with a shear field) rheocasting process has been exploited. In case of secondary die casting aluminum alloy YL112, LSPSF allowed for preparation of sound semi-solid slurry in 15-20s that fully meet the production rate of HPDC, the primary α-Al exhibiting a mean equivalent diameter of 70 μm and shape factor of 0.93, without any entrapped eutectic. Compared to conventional HPDC, RDC improves microstructures in castings. Secondary solidification of semi-solid slurry takes place uniformly throughout the entire cavity, producing an extremely fine and uniform microstructure. The experimental results show the RDC 380 alloy has much improved integrity and mechanical properties, particularly elongation, and heat treatment can be used to enhance the mechanical properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.