Microstructure and forming quality of friction stir welding joints of 7075Al and AZ31BMg with different welding parameters were analyzed. The results show that, good welded joint is obtained when the rotating frequency is 13 r/s and the welding speed is 30 mm/min. An irregular area is formed in the welding center. Meanwhile, the river pattern and eddy-like distribution are found in the weld nugget zone. Besides, brittle intermetallic compounds Al12Mg17 and Al3Mg2 are found in the welded joint. They cause the increase of microhardness of welded joint. The maximum tension stress of welded joint is 112MPa.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.