Abstract
A new severe plastic deformation (SPD) method called C shape equal channel reciprocating extrusion (CECRE) was developed to fabricate fine grained AZ31 Mg alloys. The results show that homogeneous microstructure with mean grain size of 3.6 μm is obtained as the accumulated true strain is increased to 11. Strain localization leading to dynamic recrystallizaion (DRX) occurring is the main reason for grain refinement during CECRE process. At the same time, the hardness of AZ31 alloy increases from 62.6 of as-extruded to 74.6 of CECRE 4 passes.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.