Abstract

Cerium phosphate powders were synthesized by direct solid liquid reaction of cerium dioxide and phosphate acid at the Ce: P ratio of 1∶1. Phase-pure and fine grain size CePO4 powers could be obtained by calcining the as received powders at the temperature higher than 600°C. It is demonstrated that the grain size and morphology of the CePO4 powders were calcined at various temperatures. An interesting layered crystal structure and a series of microcracks that cross and occur along the extrusion stress direction on the extruded surface inside CePO4 were observed. The ductility and machinability of CePO4 ceramic are attributed to the layered structure. Continuous machining debris was observed on the turned surface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.