Abstract

The as-cast and the pre-annealed Zr65Al7.5Ni10Cu12.5Ag5 bulk metallic glasses were rolled at room temperature to different deformation degrees, and the microstructure and microhardness were examined. It is revealed that no phase transformation occurs in the as-cast/rolled specimen except for localized shear bands, indicating that the material has a good structural stability against plastic deformation. When the glass is pre-annealed in the supercooled liquid region for a short time, however, the stability deteriorates significantly. In this case, rolling deformation results in nanocrystallization in the specimen. The pre-annealed glass has less free volume than the as-cast glass, but it does not exhibit a quicker increase in free volume content during the rolling, suggesting that free volume is prone to annihilate at the crystal/glass interfaces. With nanocrystallization occurred, the microhardness of the pre-annealed specimen decreases at a slower rate than that of the as-cast one during rolling deformation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.