► Zirconia fiber was used as reinforcing phase. ► The flexural strength and fracture toughness were obviously increased. ► Toughening mechanisms are transformation toughening, fiber pull-out, bridging and branching. ZrB 2 –SiC–ZrO 2f ceramic was fabricated by hot-pressing at 1850 °C for 1 h under a uniaxial load of 30 MPa in vacuum. The ZrB 2 –SiC–ZrO 2f ceramic thus produced showed excellent fracture toughness due to the addition of ZrO 2 fiber. The increase in toughness was attributed mainly to the addition of the ZrO 2 fiber, which could enhance fiber pull-out, crack bridging and crack branching. In addition, the stress-induced transformation toughening was also considered to be main reason for the improvement in toughness.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.