Ti (C,N)-TiB2-WC composite ceramic tool materials with sintering aids such as Ni and Mo were fabricated at a temperature of 1550 °C for 1h sintering duration time in vacuum by a hot-press technique. The microstructure and mechanical properties were investigated. The composite ceramic tool materials were analyzed by means of scanning electron microscope (SEM), X-ray diffraction (XRD) and energy dispersive spectrometry (EDS). The main phases were composed of Ti (C, N), TiB2,WC and MoC, which indicated that no severe chemical reactions occurred in the composite. The flexural strength, fracture toughness and hardness of Ti (C,N)- 20 wt.%TiB2-WC ceramic material were 795.7 MPa, 6.4 MPa·m1/2and 19.2 GPa respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.