In this study, novel CrCoNi–Al2O3 composites with 2.5–7.5 wt% Al2O3 were prepared by mechanical alloying (MA) plus rapid spark plasma sintering (SPS) method, and their microstructure and mechanical properties were systematically investigated. The results demonstrate that the Al2O3 nanoparticles are distributed homogeneously in the CrCoNi medium entropy alloy (MEA) matrix with ultra-fine grain size (≤0.37 μm). Moreover, the composites have clean, regular and well bonded matrix/α-Al2O3 interfaces. Interestingly, a large number of nano twin bundles, large-scale 9R phase and geometrically necessary dislocations (GNDs) were formed near the matrix/α-Al2O3 interfaces. The Vickers hardnesses of the 2.5–7.5 wt% Al2O3 composites reach 521–603 HV0.3, and the compressive yield strength is 1877–2359 MPa with fracture strains of 9.3–31.6%. The yield strength of the composites is by 65.4–107.8% higher than that of the pure CrCoNi matrix, meanwhile they still have considerable ductility, which indicates composite strengthening is a feasible method to improve mechanical properties of high/medium entropy alloys. The composite includes multiply strengthening mechanisms, namely grain refinement strengthening, twin strengthening, Orowan strengthening and dislocation strengthening. The contributions of various strengthening mechanisms were quantitatively analyzed, which were well consistent with the experimental values.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.