Abstract

The effects of in-situ TiB2 particle fabricated from Al-Ti-B system via the self-propagating high-temperature synthesis (SHS) reaction technology on microstructure and mechanical properties of Mg-Sn-Zn-Al alloy were investigated. The results indicate that the size of the Mg2Sn and α-Mg+Mg32(Al,Zn)49 phase becomes coarser with the increasing content of Al-Ti-B preform, meanwhile the amount of eutectic α-Mg+Mg32(Al,Zn)49 phase increases too. The addition of Al-Ti-B is favorable toward promoting the strength of composites, but deteriorates elongation. The resulting as-extruded composite material with 4 wt.% Al-Ti-B preform exhibits good overall mechanical properties with an ultimate tensile strength of 291 MPa and an elongation over 2 %.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.