Abstract

α+β titanium alloy with a composition of Ti–6.55Al–3.41Mo–1.77Zr (mass fraction, %) was cast into bars in a graphite mould using vacuum induction skull melting furnace (ISM). The cast bars were hot swaged at 700 °C and then heat treated by two different regimes which resulted in fine and coarse lamella structures, respectively. The grain size of the as-cast structure was estimated to be 660 μm and the swaged samples obtained a very fine grain size in the range of 50 μm. The overall best combination of hardness, tensile properties, and wear resistance of the α+β titanium alloy was achieved by heat treating the samples at 1050 °C for getting fine lamellar structure. The maximum compression strength was reported for the heat treated samples at 800 °C with coarse lamella structure. The minimum wear rate was reported for the heat treated samples with fine lamellar structure and the maximum wear rate was obtained for as-cast samples due to its coarse and heterogeneity microstructure.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.