Abstract

BAS glass-ceramic composites reinforced with different volume fractions (0, 10, 20, 30, 40 vol%) of SiC whiskers were successfully fabricated by a hot-pressing method. The microstructure, whisker/matrix interface structure, phase constitution and mechanical properties of the composites have been systematically studied by means of SEM, TEM, XRD techniques as well as three-point bending tests. It was demonstrated that the incorporation of SiC whiskers could significantly increase the flexural strength and fracture toughness of BAS glass-ceramic matrixes. The celsian seeds can effectively promote the hexacelsian-to-celsian transformation in BaAl2Si2O8. The active Al2O3 added to the BAS matrix obviously reduced the amount of SiO2 in the matrix and formed needle-like mullite. The high temperature strengths of the composites were also investigated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.