Abstract
Abstract The laser braze-welding technique was aimed to join a low alloyed zinc coated steel used in automotive industry, with a deformable, aging hardenable aluminum alloy from the 6xxx series using as filler material a AlSi12 wire. The heterogeneous joint was obtained by welding of aluminum alloy with the filler wire and by brazing of molten aluminum alloy together with the filler wire on the surface of a zinc coated steel which remained in solid state. The results showed that by using a proper heat input, the zinc coated steel was brazed without a melting process by the aluminum alloy which was in liquid state. On the interface between the zinc coated steel and the welded seam, a thin layer (the thickness was 6 to 8 μm) formed consisting of star (Al-Fe-Si) or needle shape (Mg-Al-Fe-Mn) intermetallic phases.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.