Abstract

Microstructure and mechanical behaviors of AZ91 cast magnesium alloys with melt superheating and thermal rate treatment technique were studied. Alloy grains thicken at 820°C and refine at 870°C when they contains Mn element and the crucible had no coating on the internal surface. Moreover, the strengthening γ phase is more dispersive and uniform at 870°C. Thermal rate treatment significantly improved the microstructure, mechanical behaviors and casting quality of AZ91 alloy as microstructure of AZ91 alloy reserves some characteristics of the high temperature melt.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.