Two methods of pre-crushing power, hydrogen decrepitation (HD) and mechanical crushing (MC), were applied to prepare Sm (CobalFe0.28Cu0.06Zr0.02)7.84 magnets. Their microstructures and magnetic properties were investigated. Compared with a conventional MC method, the Sm2O3 content was decreased and the coercivity was enhanced from 8.67 to 24.03 kOe with an HD method. The larger grain size and less grain boundaries defects were obtained in HD magnets. In addition, the HD technology improved effective Sm content of magnets by decreasing oxidation of Sm. The effective Sm content played a significant role on microstructure and magnetic properties changes of the two kinds of magnets. In combinations with the changes of alloy composition and microstructures, the effect of HD technology on effective Sm content was discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.