Nd 15Dy 1.2Fe balAl 0.8B 6 magnet was prepared by spark plasma sintering (SPS) technique. Sintering between 810 and 830 °C and consequent tempering result in relatively high magnetic properties and sintering density, which are comparable to the conventionally sintered ones. Further increase of sintering temperature gains a slight increase in sintering density and decrease in magnetic properties. Grain size of NdFeB prepared by SPS is fine and uniform, which is much smaller than that of conventionally sintered ones. Continuous thin film of the Nd-rich phase is formed along the grain boundary and the density of magnet is increased through tempering, which is the main reason for improving the magnetic properties. Furthermore, TEM observations indicate a conversion of crystal structure of the Nd-rich phase at triple junction site after tempering.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.