Abstract

The microstructures of an Fe-31wt%Cr-23wt%Co ductile permanent magnet alloy after isothermal aging, thermomagnetic treatment, and step aging have been characterized by transmission electron microscopy and by measurement of the Curie temperature. Isothermal aging itself produces the undesirable microstructure. Aging at 600°C develops the magnetic chromium-rich phase. Aging at 600°C produces a nonmagnetic chromium-rich phase dispersed within the iron-rich phase. The effect of thermomagnetic treatment on the microstructure of the alloy is discussed in comparison with that of Alnico alloys. Step aging produces the deskable microstructure, viz., the elongated ferromagnetic phase imbedded in the paramagnetic phase.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.