Abstract
Results on yttrium oxide and yttrium silicate films elaborated by an innovative metal-organic chemical vapor deposition process combining plasma assistance and a liquid precursor supply setup are presented. Plasma assistance enables deposition at a much lower substrate temperature and the pulsed-liquid precursor source allows an accurate control of the injected reactive species. According to x-ray photoelectron spectroscopy (XPS) analyses, we show that ultrathin yttrium oxide deposition can be performed at temperature less than 380°C. Yttrium oxide films contain carbon contamination that can be reduced by increasing the deposition temperature. The plasma plays a key role in the deposition mechanisms and thus in the chemical structure of the films and of the interface. It is shown that the injection frequency, i.e., the reactive species incoming frequency, plays a significant role in the silicate and interface formation. A detailed study is presented using angle-resolved XPS. A high injection frequency limits the formation of SiO2 interfacial layer and also of the silicate and favors the growth of yttrium oxide. In addition, silicate formation also depends on the deposition temperature. Electrical results show that as-deposited film at 350°C has a low leakage current (J<10−7A∕cm2) and a high breakdown field (∼8MV∕cm).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.