Abstract

The effects of pulsed magnetic field on the solidified structure of pure Mg were investigated. Fine uniform equiaxed grains are acquired in the whole ingot from the PMF treatment, in contrast with the coarse columnar grains observed in conventional casting, and the average grain size is refined to 260 m with a 5Hz PMF treatment. The mould size also affects the grain refinement and the most suitable inner diameter of the cylindrical mould is set at 50mm. Pulsed magnetic field increases melt convection during solidification, and the violent agitation causes warmer liquid to fracture the tip of columnar dendrites or to break off dendrite branches and promote the formation of an equiaxed structure, with the broken pieces transported into the bulk liquid acting as nuclei.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.