Pb-free ferroelectric solid solution of Bi0.5K0.5TiO3 with BiCoO3 has been fabricated using a sol-gel technique, exhibiting room-temperature ferromagnetism. The optical bandgap of Bi0.5K0.5TiO3 reduced from 3.21 eV to 1.77 eV with increasing amount of BiCoO3 solid solution. The room-temperature ferromagnetism and bandgap reduction occurred due to BiCoO3 diffusion into Bi0.5K0.5TiO3, resulting in formation of solid solution. These results provide a simple approach to realize room-temperature ferromagnetism in Pb-free ferroelectric materials.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.