Abstract

Two plain carbon steel plates were joined by magnetic pulse welding process. The optimum condition was found to be 16kV discharge voltage and 0.8mm standoff distance for the present set of plates. Three distinct zones of bonding namely; solid state bonding, homogeneous liquid state bonding and liquid state bonding with pores and cracks were observed. Any appreciable changes observed were restricted within 5μm distance from the weld line. Microstructural as well as crystallographic alterations of the structures were not detected beyond 5μm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.