Abstract

The dynamic rheology and accompanying microstructure of a synthetic mesophase pitch (AR-HP) is reported. The loss modulus (G″) was found to be higher than the storage modulus (G′) at all frequencies (∼0.1 to ∼100 rad/s) and temperatures (280–305 °C) tested. The slope of the low-frequency terminal zone for G′ was found to be approximately 0.8, much lower than a value of 2 that is observed for flexible chain polymers. Cross-polarized optical microscopy with full-wave retardation plate confirmed the presence of different textures of mesophase pitch processed under different conditions. While loss moduli remained fairly unchanged, finer textures led to significantly lower storage moduli. Consistent with this trend, coarsening of the microstructure during textural relaxation led to an increase in storage moduli. Therefore, for the discotic mesophase pitch, the viscous component was found to remain unaffected by the microstructure, but the elastic modulus was dependent on the orientation of layer-planes and size of the texture.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.