Abstract
The present study concerns a detailed investigation of microstructural evolution of nickel based hardfaced coating on AISI 304 stainless steel by high velocity oxy-fuel (HVOF) deposition technique. The work has also been extended to study the effect of coating on microhardness, wear resistance and corrosion resistance of the surface. Deposition has been conducted on sand blasted AISI 304 stainless steel by HVOF spraying technique using nickel (Ni)-based alloy [Ni: 68.4 wt pct, chromium (Cr): 17 wt pct, boron (B): 3.9 wt pct, silicon (Si): 4.9 wt pct and iron (Fe): 5.8 wt pct] of particle size 45 to 60 μm as precursor powder. Under the optimum process parameters, deposition leads to development of nano-borides (of chromium, Cr2B and nickel, Ni3B) dispersion in metastable and partly amorphous gamma nickel (γ-Ni) matrix. The microhardness of the coating was significantly enhanced to 935 VHN as compared to 215 VHN of as-received substrate due to dispersion of nano-borides in grain refined and partly amorphous nickel matrix. Wear resistance property under fretting wear condition against WC indenter was improved in as-deposited layer (wear rate of 4.65 × 10−7 mm3/mm) as compared to as-received substrate (wear rate of 20.81 × 10−7 mm3/mm). The corrosion resistance property in a 3.56 wt pct NaCl solution was also improved.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.