Abstract

Present article reports the microstructure and wear behavior of grain refined and modified Al–7Si–0.3Mg (LM25) alloy. Combined grain refinement and modification is achieved by inoculating LM25 melt with various inoculation levels (0.2, 0.5 and 1.0 wt%) of a novel Al base master alloy containing Ti, C and Sr (synthesized in the authors’ laboratory) at 720 °C. The wear resistance of LM25 alloy improves with the addition of this master alloy up to 0.5 wt%. It is observed that α-Al cell size and morphology of the eutectic silicon of LM25 alloy have significant effect on the wear resistance of the alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.