Abstract

AbstractBoron carbide (B4C) is currently used in lightweight armors and high temperature materials, because it has high meting point, good hardness, low specific gravity and good mechanical properties. The sintering of boron carbide, however, is restricted by its high covalent bonding and B2O3coatings on B4C particles surface which can cause a microstructural coarsening during sintering. Therefore, it is necessary to remove B2O3film of By4C particles surface to restrict microstructural coarsening and densification of B4C. B4C ceramics were fabricated by a hot-press sintering and its sintering behavior, microstructure and mechanical properties were evaluated. The relative density of B4C ceramics were obtained by a hot-press sintering reached as high as 99% without any sintering additives. The mechanical properties of B4C ceramics was improved by a methanol washing which can remove B2O3phase from a B4C powder surface. This improvement is resulted from the formation of homogeneous microstructure because the grain coarsening was suppressed by the elimination of B2O3phase. Particularly, the mechanical properties of the sintered samples using a methanol washed powder improved compared with the samples using an as-received commercial powder.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.