Abstract

Fe -base alloys containing 5, 10, and 20 wt. % Cr were oxidized in a stream of O2 at 750 and 900°C up to 264 hr. A “sulfur decoration” method was applied to detect the cracks generated in the scale during oxidation. This method revealed frequent crack generation and its healing in the scale. In the case of low-Cr alloys, the cracks are filled up with newly formed Fe-rich oxide but may be regenerated during further oxidation. Cracks are generated in the scale on an Fe-20Cr alloy also, although this alloy is not so severely attacked because of rapid healing.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.