Abstract
The microchemistry of steel/enamel interfaces was investigated, on a nearly atomic scale, by means of X‐ray photoelectron spectroscopy. Experimental evidence is given that good adherence is characterized by a fully reacted iron silicate phase, which produces a local chemical continuity between steel and enamel, whereas bad adherence is associated with a heterogeneous mixture of an iron silicate phase plus unreacted FeO.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.