Abstract

The inter-critical heat affected zone (ICHAZ) appears to be one of the most brittle sections in the welding of high-strength micro-alloyed steels (HSLA). Following repeated heating cycles in in with temperature ranging Ac1 /Ac3, the ICHAZ will face with an evident toughness and fatigue behavior reduction especially due to martensite-austenite constituent (MA) formation. Microalloying in high strength steels causes the generation of some phases in the matrix able to increase the mechanical properties of the joint. In this paper we report an investigation related to 1000 ppm vanadium addition in the welded joint of a structural S355 steel. The inter-critical zone of ta double pass welded joint is here reproduced by dilatometer, with second peak temperature ranging 720°C-790°C. The residual austenite dependence on inter-critical temperature is analyzed and related to the hardness behavior.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.