ABSTRACTWe have studied methods of improving glow-discharge-deposited a-Si1−x Gex :H alloys deposited using silane and germane gas mixtures. Material processing methods studied include (1) varying the substrate temperature from 170° to 280°C, (2) varying the process gas composition and pressure, (3) dilution of the feed gas by hydrogen, argon, or helium, (4) enhancing etching during deposition by adding small amounts of XeF2 vapor into the process gas, and (5) postdeposition annealing and/or hydrogenation.