A trial set-up with methods for sampling, treatment and analysis of small wood chips are presented in this paper, to determine important wood and fibre properties, like basic density, dry density, volume swelling of wood, Kraft pulp yield, fibre length, fibre coarseness, fibre width, lumen width and fibre wall thickness. The required time for one sample is about 1.5 man-hour, but this requires relatively larger series and trained personnel. Acceptable measurement accuracy is achieved when the volume of the wood sample is at least 1.5 ml, except that of wood volume swelling. To gain acceptable measurement accuracy for volume swelling, the wood volume should be increased to at least 3 ml, and preferably more than 5–6 ml per sample. The level of pulp yield and wood density do not show a significant effect on the measurement accuracy for fibre cross-section dimensions. Fibre coarseness, on the other hand, has a significant influence on these accuracies. A double measurement of fibre coarseness will improve the accuracy to an acceptable level. The method presented here may, together with information about trees and growth locations, form the basis for greater insight into the mechanisms involved in development of wood and fibre properties in trees, which in turn may provide better control and utilisation of wood for pulp and paper production.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call