AbstractManufacturing complex parts by the laser sintering process requires a minimum amount of energy input for consolidation of polymer particles to occur; however too much energy can result in a decline in mechanical properties. This decrease is thought to be the result of polymer chain degradation. A stable sintering region (SSR) has been proposed to describe the optimum temperature range for successful laser sintering. This article will aim to quantify the SSR for polyamide‐12 by using thermogravimetric analysis (TGA) to provide a framework for identifying key laser sintering processing parameters. Weight loss with respect to temperature is the main measurement output of the TGA procedure. However, the precise temperature and thermal history of a material is difficult to quantify during the laser sintering process; instead an energy input approach has been developed. A degradation energy was calculated from the TGA data and was used in conjunction with a laser sintering formula called energy melt ratio to prescribe build parameters for laser sintered parts. The mechanical properties of these parts illustrated the effect of degradation at various levels of energy input. Implications for this work include optimizing the material selection process for polymer laser sintering materials beyond polyamide‐12. POLYM. ENG. SCI., 2013. © 2012 Society of Plastics Engineers

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.